Popanga kuwotcherera zitsulo, padzakhala kutuluka kwa zitsulo ngati njira yowotcherera si yolondola.Zowonongeka zofala kwambiri ndi kuphulika kotentha, kuzizira kozizira, kung'ambika kwa lamellar, kusowa kwa fusion ndi kulowa kosakwanira, stomata ndi slag.

Kuphulika kotentha.

Amapangidwa panthawi yozizira ya weld.Choyambitsa chachikulu ndi sulfure ndi phosphorous muzitsulo ndi kuwotcherera zimapanga zosakaniza za eutectic, zosakanizazo zimakhala zowonongeka komanso zolimba.Pa kuzizira kwa weld, zosakaniza za eutectic zimakhala zovuta kwambiri kuti ziphwanyike mosavuta.

Kuzizira kozizira.

Amadziwikanso kuti kuchedwa kusweka, amapangidwa kuyambira 200mpaka kutentha.Idzasweka pakangopita mphindi zingapo ngakhale masiku angapo.Chifukwa chake chikugwirizana kwambiri ndi mapangidwe apangidwe, zida zowotcherera, zosungirako, zogwiritsira ntchito ndi njira zowotcherera.

Kuphulika kwa Lamellar.

Pamene kuwotcherera kutentha utakhazikika kwa opanda madigiri 400, ena mwa mbale makulidwe ndi lalikulu ndi mkulu zonyansa zili, makamaka sulfure okhutira, ndipo ali kufanana amphamvu ndi kugubuduza malangizo pamodzi pepala la mphamvu mkulu otsika aloyi zitsulo tsankho pamene ali. kugonjetsedwa ndi mphamvu perpendicular kwa makulidwe malangizo mu ndondomeko kuwotcherera, izo adzatulutsa anagubuduza malangizo anaponda ming'alu.

Kupanda Fusion ndi Kulowa Kosakwanira.

Zomwe zimayambitsa ndizofanana, zosayenera zaukadaulo, miyeso ndi kukula kwa poyambira, kuyeretsa kosakwanira kwa poyambira ndi weld pamwamba kapena ukadaulo wowotcherera.

Stomata.

Chifukwa chachikulu chopangira porosity mu weld chimakhala ndi kugwirizana ndi zosankhidwa, zosungidwa ndi zogwiritsidwa ntchito pazitsulo zowotcherera, kusankha kwa njira zowotcherera, kuyeretsa kwa poyambira ndi chitetezo cha dziwe la weld.

Slag.

Mtundu, mawonekedwe ndi kugawa kwazinthu zopanda zitsulo zimagwirizanitsidwa ndi njira zowotcherera ndi mankhwala opangidwa ndi kuwotcherera, Flux ndi zitsulo zowotcherera.